Specifications |
|
| |
|
|
|
|
|
| |
Galvanized Steel |
|
 |
| |
Zinc mettalized coating can provide corrosion protection in rural and urban areas. Atmospheric conditions will not rust steel protected by a Zinc metallized coating. Therefore, a Zinc metallized coating does not distort the shape of the steel nor it will affect its mettallurgical structure. If the product is scratched and the base metal is revealed, zinc will sacrifys itself and protect the exposed area until it is consumed entirely. |
|
| |
| |
| Pre - painted Galvanized Steel |
| Thickness (TCT) |
: |
0.30 mm - 0.80 mm |
| Metallic Coating |
: |
Z 120 (Total on both sides) Higher or lower coating optional |
| Tensile strength |
: |
340 - 550 Mpa |
| Paint coating |
: |
RMP / SMP / PVDF |
| Paint Thickness |
: |
18 - 22 micorn on Top & 5 - 8 micron primer on bottom |
| Thickness Tolerance |
: |
As per ISI |
| Standard Followed |
: |
IS 277, ASTM A653 AS 1397 JISG3312 |
|
|
| |
| |
Galvalume Steel |
|
 |
| |
Zinc Aluminium alloy coating gives corrosion resistance and superior heat reflectivity. Galvalume Steel reflects a high percentage of heat and can withstand in any weather conditions, without surface discoloration. It is also suited for coastal areas. Bare Galvalume coating is inorganic and does not contain volatile compounds that can harm the environment. |
|
| |
| |
| Pre - Painted Galvalume / Bare Galvalume Steel |
| Thickness (TCT) |
: |
0.30 mm - 0.80 mm |
| Metallic Coating |
: |
Z 120 (Total on both sides) Higher or lower coating optional |
| Tensile strength |
: |
340 - 550 Mpa |
| Paint coating |
: |
RMP / SMP / PVDF |
| Paint Thickness |
: |
18 - 22 micorn on Top & 5 - 8 micron primer on bottom |
| Thickness Tolerance |
: |
As per ISI |
| Standard Followed |
: |
IS 277, ASTM A653 AS 1397 JISG3312 |
| Combination |
: |
55% AL, 43.4 % Zn & 1.5 - 1.6 % Si. |
|
|
| |
|
|
|
|
|